AWS klassifikasiýasy: AWS 5.9
DÜŞÜNDIRIŞ:
Dat almaýan polatdan ýasalan kebşirleme simi ýokary örtük netijeliligine, ähli pozisiýalarda kebşirlemekde gowy kebşirleme tehniki görkezijilerine eýedir. Olar senagatda giňden ulanylýar: gurluşyk gurluşlarynda, ulaglarda, köpri inženerçiliginde, dag-magdan maşynlarynda, demir ýolda, nebit turbalarynda, gaz basyşyny göterýän enjamlarda, güýç enjamlarynda we ş.m.
MODEL NOMERI WE ÖLÇEGI:
1. Zawodyň OEM hyzmaty bilen üpjünçilik.
2. Model: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi we ş.m.
3. MIG siminiň ölçegi: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4.TIG siminiň ölçegi: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.
GIRIŞ:
Biz dürli görnüşli polatdan ýasalan kebşirleme simlerini, şol sanda Mig berk kebşirleme simini, Tig steržen kebşirleme simini we suwasty ýaýly kebşirleme simini hödürleýäris, bularyň hemmesi ýokary hilli we bütin dünýäde satylýar.
308 we 309-dan başga-da, biz 304, 321, 347, 316L, 310, 2209 we 201-i hem hödürleýäris. Şeýle hem 318L, 904L, 2594, NiCrMo-3, Ni1 ýaly ýörite tehniki häsiýetnamalary hödürleýäris.
GAPLAMA:
Mig kebşirleme simlerini gaplamak (makara we baraban gaplamasy)
Diametri: 0.8 - 2.0mm
Gaplama: 1 kg/makara, 5 kg/makara, 15 kg/makara, 20 kg/makara, 100 kg/baraban, 200 kg/baraban
Tig çubugynyň kebşirleme siminiň gaplamasy (plastik turba)
Diametri: 1.0 - 5.0mm
Paket: 5 kg/paket
Suwa batýan ýaýly kebşirleme simi
Diametri: 2.5 - 5.0mm
Paket: 20 kg/paket, 25 kg/paket
Neýtral gaplama we OEM hoş geldiňiz!
DATSYZ POLAT KEŞFIRLEÝÄN SIMIŇ HIMIKI DÜZÜMI:
| Model belgisi | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
| ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
| ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
| ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
| ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
| ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
| ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
| ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
| Model belgisi | Dartgynlylyk güýji Rm (Mpa) | Çykyş güýji Rel ýa-da Rp0.2 (Mpa) | Uzalma (%) | Model belgisi | Dartgynlylyk güýji Rm (Mpa) | Çykyş güýji Rel ýa-da Rp0.2 (Mpa) | Uzalma (%) |
| 304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
| ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
| ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
| ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
| ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
| ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
| ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
| TIG we MIG poslanmaýan polatdan ýasalan kebşirleme simleriniň düzümi | ||||||||||
| YB5092-2005 | AWS | Himiki düzüm % | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | |||
| H08Cr20Ni9Mn7Si | ER307Si | 0.075 | 0.78 | 6.7 | 0.022 | 0.01 | 19.8 | 8.8 | ||
| H06Cr21Ni10 | ER308 | 0.045 | 0.45 | 1.9 | 0.02 | 0.009 | 20.8 | 9.8 | ||
| H0OCr21Ni10 | ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0.006 | 20 | 10.2 | ||
| H06Cr21Ni10Si | ER308Si | 0.045 | 0.85 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | ||
| H06Cr24Ni13 | ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0.009 | 24.3 | 13.2 | ||
| H06Cr24Ni13Si | ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0.009 | 24.7 | 13.2 | ||
| H03Cr24Ni13 | ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 | ||
| H03Cr24Ni13Si | ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 | ||
| H21Cr16Ni35 | ER330 | 0.2 | 0.38 | 1.5 | 0.022 | 0.01 | 16.5 | 34.5 | ||
| H06Cr19Ni12Mo2 | ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H06Cr19Ni12Mo2Si | ER316Si | 0.05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H03Cr19Ni12Mo2 | ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 | |
| H03Cr19Ni12Mo2Si | ER316LSi | 0.06 | 0.85 | 1.7 | 0.022 | 0.01 | 18.8 | 12.6 | 2.4 | |
| H03Cr17Ni14Mo3 | ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 | |
| H08Cr19Ni12Mo2Nb | ER318 | 0.06 | 0.42 | 1.5 | 0.022 | 0.01 | 18.5 | 11.8 | 2.3 | |
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0.022 | 0.01 | 19.8 | 33.3 | 2.8 | Nb0.7 |
| H02Cr20Ni34Mo2Cu3Nb | ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Nb0.35 |
| H08Cr20Ni10Ti | ER321 | 0.06 | 0.45 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | Ti9xC-1.0 | |
| H08Cr21 Ni10Nb | ER347 | 0.055 | 0.48 | 1.8 | 0.021 | 0.008 | 20.8 | 9.8 | Nb1xC-1.0 | |
| H12Cr26Ni21 | ER310 | 0.09 | 0.5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 | ||
| H02Cr20Ni25Mo4Cu | ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | Cu 1.80 |
| H03Cr22Ni9Mo3N | ER2209 | 0.022 | 0.5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | ER2553 | 0.027 | 0.5 | 1 | 0.025 | 0.015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | ER312 | 0.09 | 0.38 | 1.5 | 0.022 | 0.01 | 29.5 | 8.5 | ||
| H03Cr24Ni13MoL | ER309L Mo | 0.023 | 0.45 | 1.5 | 0.022 | 0.01 | 23.8 | 13.2 | 2.2 | |
| H05Cr17Ni4Cu4Nb | ER630 | 0.04 | 0.39 | 0.5 | 0.022 | 0.01 | 16.5 | 4.8 | Cu;3 Nb;0.28 | |
| H08Cr26Ni5Mo2 | ER453-ler | 0.06 | 0.3 | 0.4 | 0.022 | 0.01 | 25.8 | 4.8 | 2.1 | |
| H08Cr21Ni10Mn6 | 0.06 | 0.35 | 5.5 | 0.022 | 0.01 | 20.8 | 9.8 | |||
| H05Cr22Ni11Mn6Mo3VN | ER209 | 0.04 | 0.4 | 4.5 | 0.022 | 0.01 | 21.5 | 10.8 | 2.2 | N;0.20 V;0.18 |
“Wenzhou Tianyu Electronic Co., Ltd.” kompaniýasy 2000-nji ýylda esaslandyryldy. Biz 20 ýyldan gowrak wagt bäri kebşirleme elektrodlaryny, kebşirleme taýaklaryny we kebşirleme üçin sarp edilýän materiallary öndürmek bilen meşgullanýarys.
Esasy önümlerimiz poslamaýan polatdan ýasalan kebşirleme elektrodlaryny, uglerodly polatdan ýasalan kebşirleme elektrodlaryny, pes lehimli kebşirleme elektrodlaryny, ýüzleý kebşirleme elektrodlaryny, nikel we kobalt lehimli kebşirleme elektrodlaryny, ýumşak polat we pes lehimli kebşirleme simlerini, poslamaýan polatdan ýasalan kebşirleme simlerini, gaz bilen goralýan akustik özenli simleri, alýumin kebşirleme simlerini, suwasty ýaý kebşirlemesini, simleri, nikel we kobalt lehimli kebşirleme simlerini, bürünç kebşirleme simlerini, TIG we MIG kebşirleme simlerini, volfram elektrodlaryny, uglerod lehimleme elektrodlaryny we beýleki kebşirleme aksesuarlaryny we sarp ediş materiallaryny öz içine alýar.
“Wenzhou Tianyu Electronic Co., Ltd.” kompaniýasy 2000-nji ýylda esaslandyryldy. Biz 20 ýyldan gowrak wagt bäri kebşirleme elektrodlaryny, kebşirleme taýaklaryny we kebşirleme üçin sarp edilýän materiallary öndürmek bilen meşgullanýarys.
Esasy önümlerimiz poslamaýan polatdan ýasalan kebşirleme elektrodlaryny, uglerodly polatdan ýasalan kebşirleme elektrodlaryny, pes lehimli kebşirleme elektrodlaryny, ýüzleý kebşirleme elektrodlaryny, nikel we kobalt lehimli kebşirleme elektrodlaryny, ýumşak polat we pes lehimli kebşirleme simlerini, poslamaýan polatdan ýasalan kebşirleme simlerini, gaz bilen goralýan akustik özenli simleri, alýumin kebşirleme simlerini, suwasty ýaý kebşirlemesini, simleri, nikel we kobalt lehimli kebşirleme simlerini, bürünç kebşirleme simlerini, TIG we MIG kebşirleme simlerini, volfram elektrodlaryny, uglerod lehimleme elektrodlaryny we beýleki kebşirleme aksesuarlaryny we sarp ediş materiallaryny öz içine alýar.